Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.38 J/cm² | 6.57 ft-lb/in² | ISO 179/1eA |
NOVA Chemicals Dylark® 520XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Charpy Impact, Notched | 1.38 J/cm² @Temperature -30.0 °C |
6.57 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Conditioned) Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold... |
|||
Charpy Impact, Notched | 1.38 J/cm² | 6.57 ft-lb/in² | ISO 179 |
BASF Ultramid® TG3S BK-104 15% Glass Filled PA6 (Dry) Ultramid TG3S BK-104 is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a balance .. |