Polymer Property : Charpy Impact, Notched = 1.38 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.38 J/cm²
6.57 ft-lb/in²
ISO 179/1eA
NOVA Chemicals Dylark® 520XT Glass Reinforced Engineering Resin
Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri..
Charpy Impact, Notched 1.38 J/cm²

@Temperature -30.0 °C
6.57 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Conditioned)
Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold...
Charpy Impact, Notched 1.38 J/cm²
6.57 ft-lb/in²
ISO 179
BASF Ultramid® TG3S BK-104 15% Glass Filled PA6 (Dry)
Ultramid TG3S BK-104 is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a balance ..