Polymer Property : Charpy Impact, Notched = 52.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 11.0 J/cm²
52.3 ft-lb/in²
Partial Break; ISO 179-1/1eA
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data)
By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey..
Charpy Impact, Notched 11.0 J/cm²
52.3 ft-lb/in²
Partial Break; ISO 179-1/1eA
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data)
TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an..
Charpy Impact, Notched 11.0 J/cm²
52.3 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® BRZ 347 W PA6
Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi..
Charpy Impact, Notched 11.0 J/cm²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® FN727 BK230A Nylon 6
Zytel® FN727 BK230A is a black, impact modified, plasticizer free, very flexible polyamide 6 alloy resin having good low temperature toughness, good heat aging and good chemical resistance. Uses in..
Charpy Impact, Notched 11.0 J/cm²
52.3 ft-lb/in²
Partial; ISO 179/1eA
DuPont Performance Polymers Hytrel® 6646 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
66 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers