Mechanical Properties Metric English Comments
Charpy Impact, Notched 5.80 J/cm²

@Temperature 23.0 °C
27.6 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East)
Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T..
Charpy Impact, Notched 5.80 J/cm²

@Temperature -30.0 °C
27.6 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® EXL8454 PC COPOLYMER (Asia Pacific)
Lexan* EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color..
Charpy Impact, Notched 5.80 J/cm²

@Temperature 23.0 °C
27.6 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® FXG154 PC
FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact, Notched 5.80 J/cm²
27.6 ft-lb/in²
80*10*4mm, Cut; ISO 179/1eA
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP
SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin..
Charpy Impact, Notched 5.80 J/cm²
27.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® CL101 PBT+PC
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Charpy Impact, Notched 5.80 J/cm²
27.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific)
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Charpy Impact, Notched 5.80 J/cm²
27.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East)
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Charpy Impact, Notched 5.80 J/cm²
27.6 ft-lb/in²
ISO 179/1eA
Lubrizol ESTALOC® 59200 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Charpy Impact, Notched 5.80 J/cm²
27.6 ft-lb/in²
Partial Break
Arkema Group Appryl® 7280 Polypropylene - Polyethylene Copolymer
PP/PE copolymer colored directly or during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive i..
Charpy Impact, Notched 5.80 J/cm²
27.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® FXG154 PC (Asia Pacific)
FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.