Material Notes:
Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important properties: Good impact strengthHigh stiffnessEasy processing Application examples are structural components for furniture applications, housings for electro power tools and functional parts for automotive applications.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 90.0 MPa
13100 psi
conditioned; ISO 2039-1
170 MPa
24700 psi
dry; ISO 2039-1
Tensile Strength at Break 100 MPa
14500 psi
conditioned; ISO 527-1/-2
170 MPa
24700 psi
dry; ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
dry; ISO 527-1/-2
6.0 %
6.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 5.80 GPa
841 ksi
conditioned; ISO 527-1/-2
10.0 GPa
1450 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 8.50 J/cm²
40.4 ft-lb/in²
dry; ISO 179/1eU
9.50 J/cm²
45.2 ft-lb/in²
conditioned; ISO 179/1eU
8.00 J/cm²

@Temperature 30.0 °C
38.1 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
8.00 J/cm²

@Temperature 30.0 °C
38.1 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
dry; ISO 179/1eA
2.80 J/cm²
13.3 ft-lb/in²
conditioned; ISO 179/1eA
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
16.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
35.0 kV/mm
889 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Interior
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories