Polymer Property : Charpy Impact, Notched = 40.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 8.60 J/cm²
40.9 ft-lb/in²
ISO 179
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP
SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain..
Charpy Impact, Notched 8.60 J/cm²
40.9 ft-lb/in²
Arkema Group Kynar® FLEX 2800 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EG1N, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, impervious..