Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.710 J/cm² | 3.38 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 3216 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.710 J/cm² @Temperature -30.0 °C |
3.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra.. |
|||
Charpy Impact, Notched | 0.710 J/cm² @Temperature -30.0 °C |
3.38 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi.. |
|||
Charpy Impact, Notched | 0.710 J/cm² | 3.38 ft-lb/in² | ISO 179 |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |
|||
Charpy Impact, Notched | 0.710 J/cm² | 3.38 ft-lb/in² | |
Asahi Kasei Tenac®-C EF450 Copolymer Polyacetal Resin Applications: Automotive: Fuel Pump Module Parts Electrical and Industrial: Audio-Visual Equipment, Printer EquipmentInformation provided by Asahi Kasei |
|||
Charpy Impact, Notched | 0.710 J/cm² @Temperature -30.0 °C |
3.38 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BESHV Nylon 11, Blow Molding Grade (Conditioned) Designation ISO 1874-PA11,E,24-010Rigid grade for extrusion blow molding. Available color: natural. Additive free.Very good impact strength. Well adapted melt strength. High chemical resistance.Food.. |