Polymer Property : Charpy Impact, Notched = 24.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 5.10 J/cm²
24.3 ft-lb/in²
ISO 179
GEHR Plastics PP-30PET-F Polypropylene, 30% PET Fiber Reinforced  (discontinued **)
Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle...
Charpy Impact, Notched 5.10 J/cm²
24.3 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS
LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant.
Charpy Impact, Notched 5.10 J/cm²
24.3 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific)
Designed for outdoor telecommunications enclosure applications.
Charpy Impact, Notched 5.10 J/cm²

@Temperature 23.0 °C
24.3 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® 364 PBT
This data was supplied by SABIC-IP for the Americas region.
Charpy Impact, Notched 5.10 J/cm²
24.3 ft-lb/in²
ISO 179-1
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound
Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding..