Mechanical Properties Metric English Comments
Charpy Impact, Notched 21.0 J/cm²
99.9 ft-lb/in²
ISO.179 DN.53453
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000
PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P..
Charpy Impact, Notched 21.0 J/cm²

@Temperature -20.0 °C
99.9 ft-lb/in²

@Temperature -4.00 °F
After conditioning at 23°C/50%RH; ISO 179/Af
Arkema Group Orgalloy® LE 60 SF Polyamide Alloy
Polyamide Alloy, Film and PackagingInformation provided by Arkema Group
Charpy Impact, Notched 21.0 J/cm²
99.9 ft-lb/in²
ISO.179 DN.53453
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000
PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P..