Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.30 J/cm² @Temperature -30.0 °C |
20.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 4.30 J/cm² @Temperature -30.0 °C |
20.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 4.30 J/cm² @Temperature -30.0 °C |
20.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 4.30 J/cm² @Temperature -30.0 °C |
20.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 4.30 J/cm² @Temperature -30.0 °C |
20.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized |
|||
Charpy Impact, Notched | 4.30 J/cm² | 20.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Charpy Impact, Notched | 4.30 J/cm² | 20.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Charpy Impact, Notched | 4.30 J/cm² | 20.5 ft-lb/in² | ISO Data |
Styron Pulse® B250 ABS + Polycarbonate PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. .. |
|||
Charpy Impact, Notched | 4.30 J/cm² | 20.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Charpy Impact, Notched | 4.30 J/cm² | 20.5 ft-lb/in² | ASTM D256 |
Plenco 08218 Polyester BMC, Compression Molded PLENCO 08218 is a renumber of PlasGlas 20118. PLENCO 08218 is an 18% glass-filled polyester bulk molding compound characterized as an electrical grade, but has many outstanding properties that make .. |
|||
Charpy Impact, Notched | 4.30 J/cm² | 20.5 ft-lb/in² | ISO 179-1 |
Unitika A1030FR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 4.30 J/cm² | 20.5 ft-lb/in² | ISO 179 |
Polyram PlusTek PB841 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 4.30 J/cm² @Temperature -30.0 °C |
20.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |