Material Notes:
Impact modified Nylon 6 for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.5 %
2.5 %
50% RH; ISO 62
Water Absorption at Saturation 8.0 %
8.0 %
ISO 62
Linear Mold Shrinkage 0.012 - 0.016 cm/cm
0.012 - 0.016 in/in
ISO 2577
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527
Elongation at Break 50 %
50 %
ISO 527
Flexural Strength 85.0 MPa
12300 psi
ISO 178
Flexural Modulus 2.20 GPa
319 ksi
ISO 178
Izod Impact, Notched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
ISO 180
Charpy Impact, Notched 4.30 J/cm²
20.5 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ISO 11357
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous use
180 °C
356 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 170 °C
338 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 60250