Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.29 J/cm² | 10.9 ft-lb/in² | |
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |