Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.480 J/cm² | 2.28 ft-lb/in² | ISO 179/1eA |
Radici Radilon® ACP300 K (dry) Nylon 66 Heat stabilized mineral filledInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.480 - 0.640 J/cm² @Temperature -30.0 - -30.0 °C |
2.28 - 3.05 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.575 J/cm² Grade Count:6 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Charpy Impact, Notched | 0.480 J/cm² @Temperature -30.0 °C |
2.28 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastar DN102 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.480 J/cm² | 2.28 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 FK 1010 Nylon 6 for injection molding, 10% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.480 J/cm² @Temperature 23.0 °C |
2.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Depending on specific customer requirements either a biodegradable polymer or a polyolefin can be used as the polymeric matrix. With the brand name of F.. |
|||
Charpy Impact, Notched | 0.480 J/cm² | 2.28 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® TD542 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Charpy Impact, Notched | 0.480 J/cm² @Temperature -30.0 °C |
2.28 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastar DN001 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.480 J/cm² @Temperature 23.0 °C |
2.28 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Charpy Impact, Notched | 0.480 J/cm² @Temperature 23.0 °C |
2.28 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT 4021 Polyimide, Black, 15% Graphite (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Charpy Impact, Notched | 0.480 J/cm² | 2.28 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 Zytel FE3734 NC010 is an unreinforced lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.480 J/cm² | 2.28 ft-lb/in² | ISO R179 |
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Charpy Impact, Notched | 0.480 J/cm² @Temperature -30.0 °C |
2.28 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an.. |
|||
Charpy Impact, Notched | 0.480 J/cm² | 2.28 ft-lb/in² | |
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |
|||
Charpy Impact, Notched | >= 0.480 J/cm² @Temperature 23.0 °C |
>= 2.28 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
AKG Polymers Vision PP PPC BL10004 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Charpy Impact, Notched | >= 0.480 J/cm² @Temperature 23.0 °C |
>= 2.28 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
AKG Polymers Vision PP PPC BL5005 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Charpy Impact, Notched | >= 0.480 J/cm² @Temperature 23.0 °C |
>= 2.28 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
AKG Polymers Vision PP PPC SK3005 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Charpy Impact, Notched | >= 0.480 J/cm² @Temperature 23.0 °C |
>= 2.28 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
AKG Polymers Vision PP PPC TC3005 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Charpy Impact, Notched | 0.480 J/cm² | 2.28 ft-lb/in² | |
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Conditioned) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Charpy Impact, Notched | 0.480 J/cm² @Temperature -30.0 °C |
2.28 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Conditioned) Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be pro.. |
|||
Charpy Impact, Notched | 0.480 J/cm² @Temperature 23.0 °C |
2.28 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612
(Unverified Data**) Zytel® FE3734 NC010 is an unreinforced, lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers |