Charpy Impact, Notched 0.800 - 3.70 J/cm²
3.81 - 17.6 ft-lb/in²
Average value: 1.90 J/cm² Grade Count:3
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..