Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.48 J/cm² | 16.6 ft-lb/in² | |
Covestro Bayflex® 110-50 Polyurethane Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |