Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.100 - 26.0 J/cm² @Temperature -20.0 - 0.000 °C |
0.476 - 124 ft-lb/in² @Temperature -4.00 - 32.0 °F |
Average value: 2.91 J/cm² Grade Count:16 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |