Polymer Property : Charpy Impact, Notched = 1.99 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.99 J/cm²
9.47 ft-lb/in²
Arkema Group Rilsan® MB 3945 Nylon 11, Rotomolding Grade (Dry)
Designation ISO 1874-PA11-P,RDR,12-004Semi-rigid grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyeth..