Material Notes:
Designation ISO 1874-PA11-P,RDR,12-004Semi-rigid grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High thermal and chemical resistance. Outstanding mechanical properties. Low permeability to gas and hydrocarbon.Example applications: Oil tank, hydraulic fluid tank.ISO data provided by the manufacturer, Arkema.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 32 %
32 %
50 mm/min
Tensile Modulus 0.575 GPa
83.4 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 1.99 J/cm²
9.47 ft-lb/in²
0.490 J/cm²

@Temperature -30.0 °C
2.33 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F