Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.290 J/cm² @Temperature -30.0 °C |
1.38 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Centrex® 811 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature -30.0 °C |
1.38 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Centrex® 814 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature 23.0 °C |
1.38 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
IRPC Polimaxx Polene 1100NK Polypropylene Homopolymer CHARACTERISTICS: HIGH FLOWAPPLICATIONS: FOR INJECTION MOLDING GENERAL PURPOSE : HOUSEWARES, CLOSURES, FOOD CONTAINERS |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature 23.0 °C |
1.38 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
IRPC Polimaxx Polene N1000P Polypropylene Homopolymer APPLICATION: BASE COMPONENT FOR COLORING RESIN |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature 23.0 °C |
1.38 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
IRPC Polimaxx Polene N700P Polypropylene Homopolymer APPLICATION: BASE COMPONENT FOR COLORING RESIN |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature 23.0 °C |
1.38 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
IRPC Polimaxx Polene 1124NA Polypropylene Homopolymer CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN LOW SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM AND TUBULAR BLOW FILM WATER QUENCH CPP FILM FOR FOOD PACKAGING, CPP FILM FOR LAMINATION |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature 23.0 °C |
1.38 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
IRPC Polimaxx Polene 1125NA Polypropylene Homopolymer CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN MEDIUM SLIP AND ANTIBLOCK ADDITIVESAPPLICATIONS: CAST FILM AND TUBULAR BLOW FILM WATER QUENCH CPP FILM FOR FOOD PACKAGING, CPP FILM FOR LAMINATIO.. |
|||
Charpy Impact, Notched | 0.291 J/cm² | 1.38 ft-lb/in² | ASTM D256 |
Plenco 7321 Phenolic, Granular, Transfer Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Charpy Impact, Notched | 0.290 J/cm² | 1.38 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 600JP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Low melting point DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.290 J/cm² | 1.38 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 652SA Polybutylene Terephthalate (PBT), Low density, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.290 J/cm² | 1.38 ft-lb/in² | ISO 179-1 |
Vyncolit A2710 Glass Fiber Reinforced Novolac Phenolic Vyncolit A2710 is a glass fiber reinforced phenolic molding compound with excellent mechanical and thermal properties.Information provided by Sumitomo Bak North America, Inc. |
|||
Charpy Impact, Notched | 0.290 J/cm² | 1.38 ft-lb/in² | ISO 179-1 |
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak.. |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature -30.0 °C |
1.38 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastar EN058 PET Copolymer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature -30.0 °C |
1.38 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Dry) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
Charpy Impact, Notched | 0.290 J/cm² @Temperature -30.0 °C |
1.38 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Centrex® 825 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi.. |
|||
Charpy Impact, Notched | 0.289 J/cm² | 1.38 ft-lb/in² | ASTM D256 |
Plenco 7321 Phenolic, Nodular, Injection Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Charpy Impact, Notched | 0.290 J/cm² | 1.38 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T375J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.290 - 1.00 J/cm² | 1.38 - 4.76 ft-lb/in² | Average value: 0.471 J/cm² Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |