Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7321 Phenolic, Nodular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Flock Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7321 Phenolic, Nodular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under component file E40654. 07321 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.570 g/cc
0.0206 lb/in³
ASTM D1895
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Water Absorption 0.41 %
0.41 %
ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 69
69
ASTM D785
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 0.71 %
0.71 %
ASTM D638
Tensile Modulus 7.30 GPa
1060 ksi
ASTM D638
Flexural Strength 61.0 MPa
8850 psi
ASTM D790
Flexural Modulus 6.20 GPa
899 ksi
ASTM D790
Compressive Strength 139 MPa
20200 psi
ASTM D695
Izod Impact, Notched 0.277 J/cm
0.519 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.289 J/cm²
1.38 ft-lb/in²
ASTM D256
Impact 224
224
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C
374 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Shrinkage 0.22 %
0.22 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 6.38e+10 ohm-cm
6.38e+10 ohm-cm
ASTM D247
Dielectric Constant 4.8
4.8
ASTM D150
Dielectric Strength 9.80 kV/mm
249 kV/in
Short Time; ASTM D149
Dissipation Factor 0.059
0.059
ASTM D150
Arc Resistance 26 sec
26 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638