Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.32 J/cm² @Temperature -30.0 °C |
6.28 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Conditioned) Designation ISO 1874-PA11,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Good chemical resistanc.. |
|||
Charpy Impact, Notched | 1.32 J/cm² @Temperature -30.0 °C |
6.28 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BESVO A FDA Nylon 11 (Conditioned) Designation ISO 1874-PA11,E,22-010Rigid grade for tubes and films extrusion in food applications. Available color: natural. Additive free.Good thermal and chemical resistance. Transparency. Barrier .. |
|||
Charpy Impact, Notched | 1.32 J/cm² @Temperature 23.0 °C |
6.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |