Arkema Group Rilsan® BESVO A FDA Nylon 11 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Unreinforced
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BESVO A FDA Nylon 11 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA11,E,22-010Rigid grade for tubes and films extrusion in food applications. Available color: natural. Additive free.Good thermal and chemical resistance. Transparency. Barrier properties.Food contact approval FDA 21 CFR 175.1500 and EEC directive N 90/128. UL classification: UL94 HB; RTI(C) 65/65/65Example applications: Sausage casing.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Melt Flow 5.7 g/10 min

@Load 10.0 kg,
Temperature 235 °C
5.7 g/10 min

@Load 22.0 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.0 MPa
5370 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 6.0 %
6.0 %
50 mm/min
Tensile Modulus 1.28 GPa
186 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 1.49 J/cm²
7.09 ft-lb/in²
1.32 J/cm²

@Temperature -30.0 °C
6.28 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 85.0 µm/m-°C

@Temperature 20.0 °C
47.2 µin/in-°F

@Temperature 68.0 °F
Melting Point 183 °C
361 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
Vicat Softening Point 160 °C
320 °F
50°C/hr; 50N
Electrical Properties Metric English Comments
Dielectric Strength 30.0 kV/mm
762 kV/in