Polymer Property : Charpy Impact, Notched = 0.860 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.860 J/cm²
4.09 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® C 52G1 V25 Grey R7035 (XC 1329/A) PA6, Conditioned
Description: Polyamide 6, Glass-filled, glow-wire modified, color stabilized, lubricated for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Application..
Charpy Impact, Notched 0.860 J/cm²
4.09 ft-lb/in²
ISO 179/1eA
Polyplastics FR-PET® B9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
Charpy Impact, Notched 0.860 J/cm²
4.09 ft-lb/in²
GB-1043
Zhejiang Juner PA-A6-4 Non-Reinforced
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Charpy Impact, Notched 0.860 J/cm²
4.09 ft-lb/in²
ISO 179/1eA
Polyplastics FR-PET® C9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
Charpy Impact, Notched 0.860 J/cm²
4.09 ft-lb/in²
Biomer P240 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..