Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zhejiang Juner PA-A6-4 Non-Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner PA-A6-4 Non-Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
GB-1033
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.3 MPa
11600 psi
GB-1040
Elongation at Break 5.0 %
5.0 %
GB-1040
Flexural Strength 110.5 MPa
16030 psi
GB-9341
Flexural Modulus 3.20 GPa
464 ksi
GB-9341
Charpy Impact, Notched 0.860 J/cm²
4.09 ft-lb/in²
GB-1043
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
GB-1634
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
GB-1410
Comparative Tracking Index 575 V
575 V
GB4207
Processing Properties Metric English Comments
Processing Temperature 220 - 250 °C
428 - 482 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 110 - 120 °C

@Time 14400 - 18000 sec
230 - 248 °F

@Time 4.00 - 5.00 hour
Injection Pressure 80.0 - 120 MPa
11600 - 17400 psi
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved