Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.173 J/cm² | 0.823 ft-lb/in² | ASTM D256 |
Plenco 3597 Phenolic, Granular, Injection Molded PLENCO 03597 is a mineral filled phenolic molding compound offering excellent flammability ratings even at thin cross sections, along with excellent arc and comparative track resistance values. UL r.. |