Polymer Property : Charpy Impact, Notched = 0.173 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.173 J/cm²
0.823 ft-lb/in²
ASTM D256
Plenco 3597 Phenolic, Granular, Injection Molded
PLENCO 03597 is a mineral filled phenolic molding compound offering excellent flammability ratings even at thin cross sections, along with excellent arc and comparative track resistance values. UL r..