Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.330 - 0.740 J/cm² @Temperature -30.0 - -30.0 °C |
1.57 - 3.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.497 J/cm² Grade Count:3 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |