Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.560 J/cm²
2.66 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® ST35G6 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b..
Charpy Impact, Notched 0.560 J/cm²
2.67 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Charpy Impact, Notched 0.560 J/cm²
2.67 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Charpy Impact, Notched 0.560 J/cm²
2.66 ft-lb/in²
ISO 179
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA)
High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Charpy Impact, Notched 0.560 J/cm²
2.67 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® C5315 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.560 J/cm²

@Temperature 23.0 °C
2.66 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT 3012 Polyimide, Ochre Brown (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Charpy Impact, Notched 0.560 J/cm²
2.67 ft-lb/in²
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned)