Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Glass Bead Filled
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforced isotropic performances. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Low coefficient of linear expansion.Example applications: Mechanical parts with dimensional precision.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Melt Flow 70.8 g/10 min

@Load 2.16 kg,
Temperature 235 °C
70.8 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.0 MPa
5660 psi
50 mm/min
Elongation at Break 32 %
32 %
Nominal Strain; 50 mm/min
Elongation at Yield 6.0 %
6.0 %
50 mm/min
Tensile Modulus 1.72 GPa
249 ksi
1 mm/min
Charpy Impact Unnotched 4.72 J/cm²
22.5 ft-lb/in²
4.95 J/cm²

@Temperature -30.0 °C
23.6 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.560 J/cm²
2.67 ft-lb/in²
0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
Melting Point 174 °C
345 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Vicat Softening Point 160 °C
320 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
Dielectric Strength 40.0 kV/mm
1020 kV/in
Comparative Tracking Index 600 V
600 V