Polymer Property : Charpy Impact, Notched = 0.281 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.281 - 0.450 J/cm²
1.34 - 2.14 ft-lb/in²
Average value: 0.357 J/cm² Grade Count:3
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..
Charpy Impact, Notched 0.281 J/cm²
1.34 ft-lb/in²
ASTM D256
Plenco 7487 Phenolic, Granular, Transfer Molded
PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple..
Charpy Impact, Notched 0.281 J/cm²
1.34 ft-lb/in²
ASTM D256
Plenco 7556 Phenolic, Briquette, Injection Molded
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component..