Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7556 Phenolic, Briquette, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7556 Phenolic, Briquette, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.870 g/cc
0.0314 lb/in³
ASTM D1895
Density 1.82 g/cc
0.0658 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0021 cm/cm
0.0021 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 95
95
ASTM D785
Tensile Strength, Ultimate 72.0 MPa
10400 psi
ASTM D638
Elongation at Break 0.67 %
0.67 %
ASTM D638
Tensile Modulus 16.8 GPa
2440 ksi
ASTM D638
Flexural Strength 127 MPa
18400 psi
ASTM D790
Flexural Modulus 15.0 GPa
2180 ksi
ASTM D790
Compressive Strength 204 MPa
29600 psi
ASTM D695
Izod Impact, Notched 0.292 J/cm
0.547 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.281 J/cm²
1.34 ft-lb/in²
ASTM D256
Impact 183
183
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Shrinkage 0.090 %
0.090 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.20e+11 ohm-cm
2.20e+11 ohm-cm
ASTM D247
Dielectric Constant 6.2
6.2
ASTM D150
Dielectric Strength 8.90 kV/mm
226 kV/in
Short Time; ASTM D149
Dissipation Factor 0.027
0.027
ASTM D150
Arc Resistance 89 sec
89 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved