Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.215 J/cm²
1.02 ft-lb/in²
ASTM D256
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..
Charpy Impact, Notched 0.215 J/cm²
1.02 ft-lb/in²
ASTM D256
Plenco 4300 Phenolic, Granular, Transfer Molded
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric..
Charpy Impact, Notched 0.215 J/cm²
1.02 ft-lb/in²
ASTM D256
Plenco 6527 Phenolic, Granular, Injection Molded
PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco.