Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.208 J/cm²
0.990 ft-lb/in²
ASTM D256
Plenco 4300 Phenolic, Granular, Compression Molded
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric..
Charpy Impact, Notched 0.208 J/cm²
0.990 ft-lb/in²
ASTM D256
Plenco 7507 Phenolic, Granular, Compression Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..