Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.207 J/cm²
0.985 ft-lb/in²
ASTM D256
Plenco 4504 Phenolic, Granular, Compression Molded
Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c..