Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.197 J/cm²
0.938 ft-lb/in²
ASTM D256
Plenco 2369 Phenolic, Granular, Compression Molded
PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369..
Charpy Impact, Notched 0.197 J/cm²
0.938 ft-lb/in²
ASTM D256
Plenco 7021 Phenolic, Granular, Injection Molded
PLENCO 07021 is a renumber of Plaslok 7021 which is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compressio..