Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7021 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Impact Grade, Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7021 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07021 is a renumber of Plaslok 7021 which is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of switchgear parts, or where mechanical assembly requires better impact strength. PLENCO 07021 is UL recognized under component file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.460 g/cc
0.0166 lb/in³
ASTM D1895
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.0112 cm/cm
0.0112 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 86
86
ASTM D785
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 0.84 %
0.84 %
ASTM D638
Tensile Modulus 8.50 GPa
1230 ksi
ASTM D638
Flexural Strength 72.0 MPa
10400 psi
ASTM D790
Flexural Modulus 6.70 GPa
972 ksi
ASTM D790
Compressive Strength 216 MPa
31300 psi
ASTM D695
Izod Impact, Notched 0.251 J/cm
0.470 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.197 J/cm²
0.938 ft-lb/in²
ASTM D256
Impact 132
132
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 192 °C
378 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
307 °F
ASTM D648
Shrinkage 0.39 %
0.39 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.70e+14 ohm-cm
1.70e+14 ohm-cm
ASTM D247
Dielectric Constant 4.5
4.5
ASTM D150
Dielectric Strength 10.9 kV/mm
277 kV/in
Short Time; ASTM D149
Dissipation Factor 0.048
0.048
ASTM D150
Arc Resistance 77 sec
77 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved