Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 655 MPa @Temperature 104 °C |
95000 psi @Temperature 220 °F |
0°, Wet, Fill Compression |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 655 MPa @Temperature 24.0 °C |
95000 psi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |
|||
Compressive Yield Strength | 655 MPa @Temperature 24.0 °C |
95000 psi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, F3C433 Carbon Fabric Hexcel designation: F3C433-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |