Polymer Property : Compressive Yield Strength = 92.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 92.0 MPa

@Strain 5.00 %
13300 psi

@Strain 5.00 %
dry; ISO 604
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..