Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 92.0 MPa @Strain 5.00 % |
13300 psi @Strain 5.00 % |
dry; ISO 604 |
Murtfeldt Murylon® 6 Cast Nylon 6 Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia.. |