Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 483 MPa

@Temperature 23.0 °C
70100 psi

@Temperature 73.4 °F
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric
Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel
Compressive Yield Strength 483 MPa

@Temperature 24.0 °C
70100 psi

@Temperature 75.2 °F
Dry
Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F522; Fiber: 75-1/0Information provided by HexCel