Polymer Property : Compressive Yield Strength = 68000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 469 MPa

@Temperature 24.0 °C
68000 psi

@Temperature 75.2 °F
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F161; Fiber: 75-1/0Information provided by HexCel
Compressive Yield Strength 469 MPa

@Temperature 232 °C
68000 psi

@Temperature 450 °F
Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement
Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% VoidsInformation provided by HexCel
Compressive Yield Strength 469 MPa

@Temperature 93.0 °C
68000 psi

@Temperature 199 °F
Dry
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric
Hexcel designation: W3G282-42"-F593; Fiber: Amoco T-300/3kInformation provided by HexCel