Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 44.0 MPa @Temperature 22.0 °C |
6380 psi @Temperature 71.6 °F |
Dry,Cure cycle: 5 days at 22°C; ASTM D695 |
Hexcel® Redux® 830 Two-Part Epoxy Syntactic Paste Adhesive Redux® 830 is a low density, self-extinguishing, syntactic, room temperature curing, two-part, epoxy paste adhesive. Redux® 830 is supplied as a 1.5 working kit.Features: Low density; Self-extingu.. |
|||
Compressive Yield Strength | 44.0 MPa @Strain 1.00 % |
6380 psi @Strain 1.00 % |
dry; ISO 604 |
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |