Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 43.0 MPa @Strain 2.00 % |
6240 psi @Strain 2.00 % |
dry; ISO 604 |
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Compressive Yield Strength | 43.0 MPa @Strain 2.00 % |
6240 psi @Strain 2.00 % |
dry; ISO 604 |
Murtfeldt Murlubric® Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |