Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 456 MPa @Temperature 24.0 °C |
66100 psi @Temperature 75.2 °F |
|
Hexcel® F161 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F161; Fiber: 150-1/2Information provided by HexCel |