Hexcel® F161 Epoxy Resin, 1581 Glass Fabric

Category Polymer , Thermoset , Epoxy , Epoxy/Glass SMC
Manufacturer Hexcel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® F161 Epoxy Resin, 1581 Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel designation: 1581-38"-F161; Fiber: 150-1/2Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 365 MPa

@Temperature 177 °C
52900 psi

@Temperature 351 °F
424 MPa

@Temperature 24.0 °C
61500 psi

@Temperature 75.2 °F
Tensile Modulus 20.4 GPa

@Temperature 177 °C
2960 ksi

@Temperature 351 °F
27.2 GPa

@Temperature 24.0 °C
3950 ksi

@Temperature 75.2 °F
Compressive Yield Strength 276 MPa

@Temperature 177 °C
40000 psi

@Temperature 351 °F
456 MPa

@Temperature 24.0 °C
66100 psi

@Temperature 75.2 °F
Compressive Modulus 22.8 GPa

@Temperature 177 °C
3310 ksi

@Temperature 351 °F
27.4 GPa

@Temperature 24.0 °C
3970 ksi

@Temperature 75.2 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.028
Laminate
Dry Resin Content (%) 33-39
Prepreg
Fiber Volume (%) 43.4
Laminate
Flow (%) 15-25