Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 222 MPa @Temperature -54.0 °C |
32200 psi @Temperature -65.2 °F |
Dry |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |