Polymer Property : Compressive Yield Strength = 28900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 199 MPa

@Temperature 24.0 °C
28900 psi

@Temperature 75.2 °F
Dry
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel
Compressive Yield Strength 199 MPa

@Temperature -54.0 °C
28900 psi

@Temperature -65.2 °F
Dry
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel