Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 139 MPa @Temperature 24.0 °C |
20200 psi @Temperature 75.2 °F |
Wet |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |