Mechanical Properties Metric English Comments
Compressive Yield Strength 155 MPa

@Temperature 24.0 °C
22500 psi

@Temperature 75.2 °F
Warp compression
Hexcel® HexPly® F185 Epoxy Resin, K285 Kevlar Fabric
Hexcel designation: 285-38"-F185; Fiber: Kev. 49 1140Information provided by HexCel