Polymer Property : Compressive Yield Strength = 14900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 103 MPa

@Strain 5.00 %
14900 psi

@Strain 5.00 %
dry; ISO 604
Murtfeldt Murylat® Polyethylene Terephthalate
Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an..